Graphene preparation method: Electrochemical exfoliation.
• Graphene thickness by AFM: 80%, 1-3 layers.
• Sheet size by AFM: 10 μm.
• Oxygen content: 7.5% (by XPS) (C/O-ratio: 12.3).
• Raman I_D/I_G ratio: 0.4.
• Sheet resistance: 4.8 kΩ/sq.
• Typical properties of films produced thereof (after spray coating): a) 11 nm film:
90% transmittance, 1200 Ω/sq (as made). b) 20 nm film: 80% transmittance, 500 Ω/sq (as made).
Synonyms
Conductive ink,Electrochemically exfoliated graphene ink,Graphene ink
Appearance
dispersion (in DMF)
Application
An excellent material for studying electrochemistry.
Storage
room temp
Ash Content
0.2 mg/mL (PEDOT:PSS)
1 mg/mL (electrochemically exfoliated graphene)
Concentration
0.2 mg/mL (PEDOT:PSS)
Form
dispersion (in DMF)
Graphene Thickness
1-3 layers
Oxygen Content
7.5% (by XPS) (C/O-ratio: 12.3).
Packaging
50 mL in glass bottle
Preparation Method
Electrochemical exfoliation.
Quality Level
100
Raman D/G Ratio
0.4
Sheet Resistance
500 Ω/sq, 20 nm film: 80% transmittance
Size
10 μm (Sheet size by AFM)