Graphene preparation method: electrochemical exfoliation.
• Graphene thickness by AFM: ∼80% 1-3 layers.• Sheet size by AFM: 5-10 μm.• Oxygen content: 5.5 at.% (C/O-ratio: 17.2).
• Raman I_D/I_G ratio: 0.25.
• Sheet resistance: 2 kΩ/sq.
• Typical properties of films produced thereof (after dilution to 0.1 mg/mL and dry transfer from PTFE-filter):
6 nm film: 91% transmittance, sheet resistance of 24.2 kΩ/sq (as made), 7.9 kΩ/sq (after 30 min, 200 °C), <1 kΩ/sq (conc. HNO3-treatment).16 nm film: 73% transmittance, sheet resistance of 7.6 kΩ/sq (as made), 1.8 kΩ/sq (after 30 min, 200 °C), <500 Ω/sq (conc. HNO3-treatment).
Synonyms
Conductive ink,Electrochemically exfoliated graphene ink,Graphene ink
Molecular Weight
12.01
Canonical SMILES
[C]
InChI
InChI=1S/C
InChI Key
OKTJSMMVPCPJKN-UHFFFAOYSA-N
Boiling Point
Varies by solvent
Melting Point
Varies by solvent
Density
Varies by solvent
Appearance
dispersion (in NMP)
Application
• Graphene-based composites • Sensors • Biomedicines • Nanodevices
Storage
room temp
Concentration
10 mg/mL
Form
dispersion
Graphene Content
1 wt. %
Oxygen Content
5.5 at%
Packaging
50 mL in glass bottle
Preparation Method
electrochemical exfoliation
Quality Level
100
Raman D/G Ratio
0.25
Sheet Resistance
<103 Ω/sq (graphene)
Size
5-10 μm
Thickness
1-10 nm , graphene
True Density
0.9-1.1 g/mL at 25 °C